Mechanical Properties of Oued Chebeika 002 Bundle
Bhatt, Suraj; Garvie, Laurence A. J.; Hoover, Christian G. NASA Planetary Data System, published: 13 April 2026 LINK (OPEN ACCESS) “This bundle provides nanoindentation measurements, associated wavelength dispersive spectroscopy point analyses, wavelength dispersive spectroscopy maps,…
Nanoindenting the Chelyabinsk meteorite to learn about impact deflection effects in asteroidsOPEN ACCESS
Carles E. Moyano-Cambero, Eva Pellicer, Josep M. Trigo-Rodríguez, Iwan P. Williams, Jürgen Blum, Patrick Michel, Michael Küppers, Marina Martínez-Jiménez, Ivan Lloro, Jordi Sort Astrophysical Journal (2017) PDF (OPEN ACCESS) abstract Update (24 January 2017): LINK…